MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Baytec® SPR-066A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec SPR-066A is a two-component, 100%-solids spray system with a Shore hardness of 66A.*

Properties / Applications: Baytec SPR-066A is a two-component, 100%-solids spray system with a Shore hardness of 66A.* The isocyanate component is a modified diphenylmethane diisocyanate (MDI) prepolymer, and the polyol component is a polyether polyol blend. The system has added UV stabilizers and is used in spray applications to improve the corrosion, weather, and abrasion resistance of metal, concrete, wood, plastic, PVC, and porous organic and inorganic materials. In-mold spray application is also possible. Typical applications are liners for dump bodies, garbage trucks, pipes, and tanks, as well as protective layers for flexible foam, wood, and industrial surfaces. This system is also available as a grey/black-pigmented system, Baytec SPR-166A (product code U832). As with any product, use of Baytec SPR-066A in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
 1.03 g/ccPolyol
 1.09 g/ccIsocyanate
Viscosity 2100 cPPolyol
 2500 cPIsocyanate
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65ASTM D2240
Tensile Strength at Break 4.14 MPaASTM D412
Tensile Stress at Strain 2.28 MPa
@Strain 200 %
ASTM D412
 3.10 MPa
@Strain 300 %
ASTM D412
 6.14 MPa
@Strain 100 %
ASTM D412
Elongation at Break 500 %ASTM D412
Compressive Strength 0.345 MPa
@Strain 5.0 %
ASTM D575
 0.621 MPa
@Strain 10 %
ASTM D575
 1.45 MPa
@Strain 25 %
ASTM D575
Tear Strength 80.0 pliSplit Tear; ASTM D1938
 190 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 350
@Load 1.00 kg
H-18; ASTM D4060
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 14.4 kV/mmASTM D419
Arc Resistance 123 secASTM D492
 
Thermal PropertiesOriginal ValueComments
Flash Point 180 °CPolyol
 216 °CIsocyanate
 
Processing PropertiesOriginal ValueComments
Gel Time 0.250 - 0.750 min
 
Descriptive Properties
AppearanceWhite liquidPolyol
 Yellowish liquidIsocyanate
Content9.8%NCO, Isocyanate
Hydroxyl number[mg KOH/g], Polyol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Pluracol® 922 Rigid Polyol
Overview of materials for PVC, Foam Grade
Polyplastics Duranex® CRN7830 Polybutylene Terephthalate (PBT), Lower noise, 30% GF filled
SMAC SMACSONIC® Carbon ST Noise and Vibration Damping
BASF Pluracol® 736 Rigid Polyol

PCOVEST0262 / 202045

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.