MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
VICTREX™ PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Product Description:

High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food contact compliant, colour natural/beige.

Typical Application Areas:

Complex geometries with thinner cross sections or longer flow lengths where higher strength in a static system is required. Low coefficient of thermal expansion. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Information Provided by Victrex.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccCrystalline; ISO 1183
Water Absorption at Saturation 0.30 %
@Temperature 23.0 °C
ISO 62-1
 0.45 %
@Temperature 100 °C
ISO 62-1
Viscosity 200000 cP
@Temperature 400 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 cm/cm360°C nozzle, 180°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm370°C nozzle, 180°C tool; ISO 294-4
Spiral Flow 16.0 cm
@Thickness 1.00 mm
Mold Temp: 180°C, Melt Temp: 370°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
@Temperature 23.0 °C
ISO 868
Tensile Strength at Break 45.0 MPa
@Temperature 275 °C
ISO 527
 60.0 MPa
@Temperature 225 °C
ISO 527
 80.0 MPa
@Temperature 175 °C
ISO 527
 130 MPa
@Temperature 125 °C
ISO 527
 195 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 2.4 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 12.0 GPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 75.0 MPa
@Temperature 275 °C
ISO 178
 115 MPa
@Temperature 175 °C
ISO 178
 210 MPa
@Temperature 125 °C
ISO 178
 290 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 11.5 GPa
@Temperature 23.0 °C
ISO 178
Compressive Strength 55.0 MPa
@Temperature 250 °C
ISO 604
 160 MPa
@Temperature 120 °C
ISO 604
 250 MPa
@Temperature 23.0 °C
ISO 604
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
ISO 180/U
Charpy Impact Unnotched 4.50 J/cm²
@Temperature 23.0 °C
ISO 179/1U
Charpy Impact, Notched 0.750 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.3
@Frequency 1000 Hz,
Temperature 23.0 °C
IEC 60250
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Dissipation Factor 0.0040
@Frequency 1e+6 Hz,
Temperature 23.0 °C
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 20.0 µm/m-°C
@Temperature >=143 °C
Above Tg; ISO 11359
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 110 µm/m-°C
@Temperature <=143 °C
Above Tg; ISO 11359
Thermal Conductivity 0.300 W/m-K
@Temperature 23.0 °C
Average; ISO/CD 22007-4
 0.350 W/m-K
@Temperature 23.0 °C
Along flow; ISO 22007-4
Melting Point 343 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 335 °CISO 75A-f
Glass Transition Temp, Tg 143 °COnset; ISO 11357
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 100 °CHopper Temperature
Rear Barrel Temperature 355 °C
Middle Barrel Temperature 360 °C
Front Barrel Temperature 365 °C
Nozzle Temperature 370 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
@Time 10800 - 18000 sec
 120 - 150 °C
@Time 10800 - 18000 sec
 
Descriptive Properties
Gate>2 mm or 0.5 x part thickness
Runner>3.5mmmanifold
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
VICTREX™ PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Evonik VESTAKEEP® 4000GF30 PEEK

PVICTA57 / 99735

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.