MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
Categories: Carbon; Graphite

Material Notes: GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include: electrical isolation of pipelines and equipment; and use with sulfuric acid, nitric acid, and other strong oxidizing chemicals. Surface identifiable, UCAR®-323 is branded with the GRAFOIL® grade and source guarantee. The advantages of UCAR®-323 are: more than 5 times the tensile strength of the market leader PTFE; extremely tolerant to process changes (temperature & pressure); design and material give up 14 times the sealability rate; 70% less creep; absorption rate of less than 0.1%; and maintains a higher bolt torque retention and a better seal in applications of thermal cycling.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.30 g/cc
Thickness 790 micronsStandard
 1570 micronsStandard
 3180 micronsStandard
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12000 psi
Compression Set 30 %
@Pressure 34.5 MPa
after 5000 psi load
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 250 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 245 °CContinuous
Minimum Service Temperature, Air -200 °C
 
Descriptive Properties
"m" Factor3
"y" Stress (psi)2200
Coefficient of Thermal Conductivity (k)0.18
Compressibility (%)3at 5000 psi load

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sinotek Materials Packing PTFE Braided with Graphite
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting
Copper, Cu; Cold-Worked
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting

CGRAF942 / 107346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.