MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: General Notes on Saint Gobain SPECIALTY SERIES Belting Products:
Dimensional Stability: Width rigidity as well as length stability is maintained by CHEMFAB Specialty Series belting in continuous use at temperatures up to 600°F. Under normal operating tensions (3 to 10 pounds per inch of width), CHEMFAB Specialty Series holds its elongation and shrinkage to less than 1%.
Release Properties: The release properties of CHEMFAB Specialty Series equal or exceed those of any other available belting material. The PTFE coating makes CHEMFAB Specialty Series unique in its low coefficient of friction.
Chemically Resistant: The PTFE coating encapsulates the Nomex belting carcass and enhances its useful service life.
Dynamic Strength: CHEMFAB Specialty Series's durability, coupled with low overall belt weight, allows optimal production speed with decreased power requirements.
Temperature Resistant:CHEMFAB Specialty Series belting can be operated continuously at temperatures up to 600°F and will still maintain 100% of its original profile.
Fabrication Technology: Saint-Gobain Performance Plastics belt seams have been specifically engineered to reduce the flex fatigue failure. Substantially reduced flex fatigue means longer belt life.

Notes on 1584G PTFE Coated Fiberglass Conveyor Belting:
As part of the Chemfab® Specialty Series, this product is designed for applications requiring high strength and low elongations, such as heavy weight belting. These styles are woven and coated to produce specific textures and to resist ridging, puckering, and creasing. The weave style is Satin. The substrate is fiberglass and the coating material is PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.037 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.155 g/cc0.04171 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Elongation at Yield <= 1.0 %<= 1.0 %Value given for Warp/Longitudinal Elongation at a loading of 40 lbs/in.
Tear Strength Test 100100Lbs./In. Propagation Tear Strength in fill/transverse direction
 120120Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 131 kN/m750 pliTensile Strength (Fill)
 193 kN/m1100 pliTensile Strength (Warp)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C600 °F
 
Descriptive Properties
Weight (oz/yd^2)32

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
Sinotek Materials Packing PTFE Braided with Graphite
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting

CSTGQZ102 / 2231

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.