Nitrile Butadiene Rubber (NBR) 62-72 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5509 Grade C (inactive for new design). Applications: Synthetic rubber resistant to engine lubricating oils, greases and fuels. |