MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Europlex® 99510 Film Transparent Polycarbonate Based Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: EUROPLEX® Film 99510 is a highly transparent film made from polycarbonate with special UV stabilization. It has a high-gloss surface, is inherently rigid and highly impact-resistant in a temperature range between -25 °C and 135 °C. It is resistant to weak acids and saturated aliphatic hydrocarbons.

Specific Notes for this Material: EUROPLEX® Film 99510 is employed for scales, nameplates, signs, covers, glazing, safety helmet shells, protective goggles and visors as well as for model making.

Information provided by degussa.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 60.0 MPano direction given; ISO 527
Film Elongation at Break, MD >= 50 %no direction given; ISO 527
Film Elongation at Yield, MD 6.0 %no direction given; ISO 527
Tensile Modulus 2.30 GPaISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmNo thickness given; IEC 250
Surface Resistance 1.00e+13 ohmIEC 250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 250
 0.040
@Frequency 100 Hz
IEC 250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
DIN 53752A
Specific Heat Capacity 1.30 J/g-°C
Vicat Softening Point 151 °CISO 306, Method B 50
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Yellow Index <= 1.6 %ASTM D1925
Transmission, Visible 90 %DIN 5036
 
Descriptive Properties
Birefringence1.58
Pencil HardnessHBASTM D3363

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Apec® FR1892 High-Heat Polycarbonate
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade
Celanese SO.F.TER Styrofor® HI-V0 Self Extinguishing Polystyrene, Flame Resistant
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Eastman Saflex® 0.030 inch Clear Protective Interlayer PVB Film for Glass Laminates

PHUK005 / 47139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.