MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.

Tarnamid® has the following main properties:

  • High mechanical strength, rigidity and hardness
  • High impact strength
  • High vibration damping capacity
  • Good fatigue strength
  • Very good sliding properties, abrasion resistance, low coefficient of friction
  • High thermal resistance, admissible temperature of continuous operation from -60°C to +150°C
  • High chemical resistance, particularly to organic solvents, oils, lubricants and fuels
  • Considerable moisture absorption influencing mechanical and electrical properties
  • Self-extinguishing properties (fire retardant properties)
  • Good electro-insulating properties
  • Good optical properties, relatively good transparency of molded pieces with thickness below 3.2 mm made from natural Tarnamid® (not dyed and not compounded)
  • Can be used for the production of goods coming into contact with food (grades fulfilling requirement of European Union Directive No 2002/72/EEC) with latest amendments

Information provided by Azoty Tarnow™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccISO 1183
Water Absorption 1.8 %
@Time 86400 sec
1.8 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 275 °C
50 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness  60.0 MPa
@Load 36.5 kg
8700 psi
@Load 80.5 lb
cond.; ISO 2039-1
 140 MPa
@Load 36.5 kg
20300 psi
@Load 80.5 lb
dry; ISO 2039-1
Tensile Strength, Yield 45.0 MPa6530 psicond.; ISO 527
 78.0 MPa11300 psidry; ISO 527
Elongation at Break 70 %70 %dry; ISO 527
 280 %280 %cond.; ISO 527
Tensile Modulus 0.100 GPa14.5 ksicond.; ISO 527
 2.80 GPa406 ksidry; ISO 527
Flexural Strength 28.0 MPa4060 psicond.; ISO 178
 82.0 MPa11900 psidry; ISO 178
Charpy Impact Unnotched NBNBISO 179 1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²dry; ISO 179 1eA
 1.20 J/cm²5.71 ft-lb/in²cond.; ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmcond.; IEC 93
 1.00e+15 ohm-cm1.00e+15 ohm-cmdry; IEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmcond.; IEC 93
 1.00e+15 ohm1.00e+15 ohmdry; IEC 93
Dielectric Strength 30.0 kV/mm762 kV/inIEC 243-1
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °Fcond.; ISO 75
 60.0 °C140 °Fdry; ISO 75
Vicat Softening Point 195 °C
@Load 5.10 kg
383 °F
@Load 11.2 lb
ISO 306
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
PN-EN-60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 290 °C446 - 554 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F80 - 90°C is recommended
Drying Temperature 75.0 - 100 °C
@Time 7200 - 14400 sec
167 - 212 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Injection Pressure 80.0 - 130 MPa11600 - 18900 psi80 MPa is recommended

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Europlex® 99510 Film Transparent Polycarbonate Based Film
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural
Solvay ThermalGraph® EWC-300X Fabric
LyondellBasell Lupolen V 2520 J Ethylene Vinyl Acetate, Film Grade

PZAK903 / 121855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.