MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay JAGUAR® EXCEL Surfactant
Categories: Fluid

Material Notes: Description: Clear grade with excellent wet combing and detangling benefits. Recommended for use in a broad range of conditioning shampoos.

Chemical Name: Guar Gum Derivative

C.T.F.A./I.N.C.I. Name: GUAR HYDROXYPROPYLTRIMONIUM CHLORIDE

CAS: 65497 – 29 – 2

Solubility: Soluble in water at 20°C. Insoluble in non polar solvent.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: JAGUAR EXCEL provides good substantivity together with no build up on hair. It allows development of transparent foaming formulations, thanks to its good compatibility with anionic and amphoteric surfactants commonly used in personal care products. JAGUAR EXCEL provides excellent wet-combing and wet-feel properties. It enhances as well the deposition of actives such as silicones, oils, anti-dandruff agents on hair. Ideal for transparent or opaque conditioning shampoos and cream rinses for coloured or damaged hair. Recommended use levels: 0.1 – 0.3%

Note: Viscosity develops within 15 minutes after JAGUAR EXCEL has been dispersed into water under stirring. More rapid viscosity development can be obtained by acidifying to pH 3,5-5 (with citric acid, for example).

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 g/cc0.0271 lb/in³
pH 8.5 - 10.58.5 - 10.51% aq. Sol.; AN 2131
Brookfield Viscosity 300 - 1000 cP300 - 1000 cP1% at pH5, RVT N°2 at 20 rpm; AN2131
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 82 %
@Wavelength 600 nm
>= 82 %
@Wavelength 600 nm
0.5% at pH=5, cell 1cm; AN 1010
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 11 %<= 11 %AN 3068
 
Descriptive Properties
AppearanceFine yellow powder
CompositionCoiformsNegative, AN9011
 Enterobacteria and Gram negative bacteriaNegative, AN9013
 Molds and yeasts<100 cfu/g, AN9003
 Plate Count<1000 cfu/g, AN9011
 Pseudomonas aeruginosaNegative, AN9002
 Staphylococcus AureusNegative, AN9002
OdorSlight, characteristic
Substitution levelcationic0.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD176 / 137407

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.