MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Haynes Hastelloy® B-2 alloy, sheet and plate, 2.5-8.9 mm thick, heat treated at 1066°C, rapid quenched  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Excellent resistance to HCl, also withstands hydrogen chloride, sulfuric, acetic and phosphoric acids, excellent resistance to pitting, to stress corrosion cracking and to knife-line and heat-affecting zone attack. B-2 is NOT recommended in the presence of ferric or cupric salts as these salts may cause rapid corrosion failure. Ferric or cupric salts may develop when HCl acid contacts Iron or Copper.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: ASME SB-626, UNS N10665, ASME SB-333, ASME SB-335, ASME SB-619, ASME SB-622
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 9.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 163Converted from Rockwell B hardness.
Hardness, Knoop 181Converted from Rockwell B hardness.
Hardness, Rockwell B 95
Hardness, Vickers 220Converted from Rockwell B hardness.
Tensile Strength, Ultimate 894 MPa
 806 MPa
@Temperature 427 °C
 823 MPa
@Temperature 316 °C
 849 MPa
@Temperature 204 °C
Tensile Strength, Yield 412 MPa
@Strain 0.2 %
 310 MPa
@Strain 0.2 %,
Temperature 427 °C
 328 MPa
@Strain 0.2 %,
Temperature 316 °C
 350 MPa
@Strain 0.2 %,
Temperature 204 °C
Elongation at Break 61 %in 50.8 mm
 59 %
@Temperature 204 °C
in 50.8 mm
 60 %
@Temperature 316 °C
in 50.8 mm
 60 %
@Temperature 427 °C
in 50.8 mm
Modulus of Elasticity 217 GPaRT
 117 GPa
@Temperature 1000 °C
 134 GPa
@Temperature 900 °C
 149 GPa
@Temperature 800 °C
 159 GPa
@Temperature 700 °C
 167 GPa
@Temperature 600 °C
 173 GPa
@Temperature 500 °C
 179 GPa
@Temperature 400 °C
 185 GPa
@Temperature 300 °C
 191 GPa
@Temperature 200 °C
 199 GPa
@Temperature 100 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000137 ohm-cm
@Temperature 0.000 °C
 0.000138 ohm-cm
@Temperature 100 °C
 0.000138 ohm-cm
@Temperature 200 °C
 0.000139 ohm-cm
@Temperature 300 °C
 0.000139 ohm-cm
@Temperature 400 °C
 0.000141 ohm-cm
@Temperature 500 °C
 0.000146 ohm-cm
@Temperature 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µm/m-°C
@Temperature 20.0 - 93.0 °C
 10.8 µm/m-°C
@Temperature 20.0 - 204 °C
 11.2 µm/m-°C
@Temperature 20.0 - 316 °C
 11.5 µm/m-°C
@Temperature 20.0 - 427 °C
 11.7 µm/m-°C
@Temperature 20.0 - 538 °C
Specific Heat Capacity 0.373 J/g-°C
@Temperature 0.000 °C
 0.389 J/g-°C
@Temperature 100 °C
 0.406 J/g-°C
@Temperature 200 °C
 0.423 J/g-°C
@Temperature 300 °C
 0.431 J/g-°C
@Temperature 400 °C
 0.444 J/g-°C
@Temperature 500 °C
 0.456 J/g-°C
@Temperature 600 °C
Thermal Conductivity 11.1 W/m-K
@Temperature 0.000 °C
 12.2 W/m-K
@Temperature 100 °C
 13.4 W/m-K
@Temperature 200 °C
 14.6 W/m-K
@Temperature 300 °C
 16.0 W/m-K
@Temperature 400 °C
 17.3 W/m-K
@Temperature 500 °C
 18.7 W/m-K
@Temperature 600 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 1.0 %
Cobalt, Co <= 1.0 %
Iron, Fe <= 2.0 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 28 %
Nickel, Ni 69 %As Remainder
Silicon, Si <= 0.10 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes Hastelloy® B-2 alloy, bright-annealed sheet, heat treated at 1149°C (2100°F), hydrogen cooled
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy
Haynes Hastelloy® B-2 alloy, plate, 9.1-51 mm thick, heat treated at 1066°C, rapid quenched
Haynes Hastelloy® C-276 alloy, solution heat treated flat products

NHAB2B / 16771

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.