Description: This product is a special silicone, which is suitable for wet-end and finishing applications Key Features - Smooth handle effects
- Distinct hydrophilic properties
- D4, D5, D6 free
- HANSA® LPW 797 is not sensitive to frost.
Key Applications Application: HANSA® LPW 797 is a concentrated emulsion of a hydrophilic polysiloxane softener which is suitable to be applied on leather and gives a smooth and soft handle, improving in the meanwhile the fullness of the fibers. HANSA® LPW 797 is appropriate as softener for all kinds of leather. Dilutions made from HANSA® LPW 797 can be applied by means of spray process/roller coater for finishing applications or in the wet-end stage. Diluting Instructions HANSA® LPW 797 can be converted into a micro or macro emulsion before use.Information provided by CHT Group |