MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT HANSA LPW 797 Silicone softener
Categories: Other Engineering Material

Material Notes: Description: This product is a special silicone, which is suitable for wet-end and finishing applications

Key Features

  • Smooth handle effects
  • Distinct hydrophilic properties
  • D4, D5, D6 free
  • HANSA® LPW 797 is not sensitive to frost.
Key Applications
  • all kinds of leather.
Application: HANSA® LPW 797 is a concentrated emulsion of a hydrophilic polysiloxane softener which is suitable to be applied on leather and gives a smooth and soft handle, improving in the meanwhile the fullness of the fibers. HANSA® LPW 797 is appropriate as softener for all kinds of leather. Dilutions made from HANSA® LPW 797 can be applied by means of spray process/roller coater for finishing applications or in the wet-end stage. Diluting Instructions HANSA® LPW 797 can be converted into a micro or macro emulsion before use.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 74 - 78 %74 - 78 %
pH 6.0 - 8.06.0 - 8.010% solution
Storage Temperature <= 60.0 °C<= 140 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Monthif properly stored in closed original containers
 
Descriptive Properties
AppearanceColorless to yellow liquid
ChemistryOrgan modified polysiloxane
IonicityNon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL331 / 314814

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.