MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or cast film equipment. In blown film equipment LD 105.30 can be drawn down to 1.0 mil gauge.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 1000 ppm
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blend Partner
  • Bread Bags
  • Display Packaging Film
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • High Clarity Film
  • High Quality Lamination
  • Lamination Film
  • Laundry Film
  • Light Duty Shrink Film
  • Produce Bags
  • Salad Bags
  • Textile Packaging
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccExxonMobil Method
Thickness 1.50 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 1000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1600 psiASTM D882
Film Tensile Strength at Yield, TD 1600 psiASTM D882
Film Elongation at Break, MD 210 %ASTM D882
Film Elongation at Break, TD 570 %ASTM D882
Puncture Energy 6.70 in-lbExxonMobil Method
Elmendorf Tear Strength MD 350 gASTM D1922
Elmendorf Tear Strength TD 180 gASTM D1922
Dart Drop Test 100 gASTM D1709
Film Tensile Strength at Break, MD 3610 psiASTM D882
Film Tensile Strength at Break, TD 3100 psiASTM D882
1% Secant Modulus, MD 31000 psiASTM D882
1% Secant Modulus, TD 37000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 232 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 5.2 %ASTM D1003
Gloss 76 %45°; ASTM D2457
Transmission, Visible 90 %clear; thickness not quantified
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade

PEXB032 / 37337

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.