Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or cast film equipment. In blown film equipment LD 105.30 can be drawn down to 1.0 mil gauge. Availability: Latin America, North America and South America Additive: - Antiblock: 1000 ppm
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Blend Partner
- Bread Bags
- Display Packaging Film
- Food packaging
- Form Fill and Seal Packaging
- Freezer Film
- High Clarity Film
- High Quality Lamination
- Lamination Film
- Laundry Film
- Light Duty Shrink Film
- Produce Bags
- Salad Bags
- Textile Packaging
Information provided by ExxonMobil Chemical |