Properties: DIDP is a clear, colourless, and odorless liquid, free of foreign materials. It is soluble in most organic solvent and in soluble in water. Application: Around 95% of DIDP is used in PVC as a plasticizer. More than half of the remaining 5% is used in the production of polymers other than PVC (e.g. rubbers). The remaining DIDP used in non-polymer application including anticorrosion paints, anti-fouling paints, lacquers, inks, adhesives and sealants. In wire and cable formulation DIDP finds wide use in 75°C THW building wire compounds and in 80°C and 90°C appliance wire insulation. In plastisol application, DIDP provide good initial viscosities and Excellent viscosity stability. Chemical Name: Di Iso Decyl Phthalate. Molecular Formula: C 26 H46 O4 Molecular Structure: C6 H4 (COOC10 H21 )2 CAS Number: 26761-40-0 EINECS NO.: 247-977-1 Information provided by KLJ Group |