MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

KLJ Group Kanatol 1001 Plasticizer
Categories: Fluid

Material Notes: Properties: DIDP is a clear, colourless, and odorless liquid, free of foreign materials. It is soluble in most organic solvent and in soluble in water.

Application: Around 95% of DIDP is used in PVC as a plasticizer. More than half of the remaining 5% is used in the production of polymers other than PVC (e.g. rubbers). The remaining DIDP used in non-polymer application including anticorrosion paints, anti-fouling paints, lacquers, inks, adhesives and sealants. In wire and cable formulation DIDP finds wide use in 75°C THW building wire compounds and in 80°C and 90°C appliance wire insulation. In plastisol application, DIDP provide good initial viscosities and Excellent viscosity stability.

Chemical Name: Di Iso Decyl Phthalate.

Molecular Formula: C 26 H46 O4

Molecular Structure: C6 H4 (COOC10 H21 )2

CAS Number: 26761-40-0

EINECS NO.: 247-977-1

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 - 0.966 g/cc
@Temperature 27.0 °C
0.960 - 0.966 g/cc
@Temperature 80.6 °F
ASTM D1045-08
Viscosity 105 - 111 cP105 - 111 cPKLJ TM-P-13-97
Molecular Weight 446 g/mol446 g/mol
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.50e+11 - 5.50e+11 ohm-cm3.50e+11 - 5.50e+11 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Boiling Point 255 °C491 °F3.5
 400 °C
@Pressure 0.101 MPa
752 °F
@Pressure 14.7 psi
IS-5298-05
Pour Point -48.0 °C-54.4 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.482 - 1.488
@Temperature 27.0 °C
1.482 - 1.488
@Temperature 80.6 °F
ASTM D1045-08
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM D1045-08
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.03%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.01%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<20Hazen, ASTM D1045-08
Content<0.1%Residual/Free Alcohol, KLJ TM-P-12-98
 >99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 248-254 mg KOH/gmEster Value, ASTM D1045-08
Volatile Loss<0.1%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ164 / 284185

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.