MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Traid Villarroya TKG® DF PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:
  • Great chemical resistance
  • Very good weldable and electrical insulation
  • Inherent flame retardant
  • Good slide and wear resistance
Industry Applications:
  • Conveyor technology
  • Electrical engineering
  • Chemical plant industry
  • Food engineering
  • Solar panels construction

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³
Water Absorption  <= 0.010 %
@Time 346000 sec
<= 0.010 %
@Time 96.0 hour
DIN EN ISO 62
 <= 0.020 %
@Time 86400 sec
<= 0.020 %
@Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 129 MPa18700 psiISO 2039-1
Tensile Strength 62.0 MPa8990 psi50 mm/min; DIN EN ISO 527-2
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; DIN EN ISO 527-2
Elongation at Break 17 %17 %50 mm/min; DIN EN ISO 527-2
Elongation at Yield 7.0 %7.0 %50 mm/min; DIN EN ISO 527-2
Modulus of Elasticity 2.20 GPa319 ksi
Flexural Strength 77.0 MPa
@Load 1.02 kg
11200 psi
@Load 2.25 lb
2 mm/min; DIN EN ISO 178
Flexural Modulus 2.10 GPa
@Load 1.02 kg
305 ksi
@Load 2.25 lb
2 mm/min; DIN EN ISO 178
Compressive Strength  16.0 MPa
@Strain 1 %,
Load 1.02 kg
2320 psi
@Strain 1 %,
Load 2.25 lb
5 mm/min; EN ISO 604
 28.0 MPa
@Strain 2 %,
Load 1.02 kg
4060 psi
@Strain 2 %,
Load 2.25 lb
5 mm/min; EN ISO 604
Compressive Modulus 1.90 GPa
@Load 1.02 kg
276 ksi
@Load 2.25 lb
5 mm/min; EN ISO 604
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²Max. 7,5j; DIN EN ISO 179-1EU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear  160 µm/m-°C
@Temperature 23.0 - 60.0 °C
88.9 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
 180 µm/m-°C
@Temperature 23.0 - 100 °C
100 µin/in-°F
@Temperature 73.4 - 212 °F
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.30 J/g-°C0.311 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 171 °C340 °FDIN 53765
Maximum Service Temperature, Air 150 °C302 °FShort term
 150 °C302 °FLong term
Glass Transition Temp, Tg -40.0 °C-40.0 °FDIN 53765
Flammability, UL94 V-0V-0DIN IEC 60995-11-10
 
Descriptive Properties
ColorWhite opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID934 / 318895

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.