MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Traid Villarroya TKG® DF PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes:
  • Great chemical resistance
  • Very good weldable and electrical insulation
  • Inherent flame retardant
  • Good slide and wear resistance
Industry Applications:
  • Conveyor technology
  • Electrical engineering
  • Chemical plant industry
  • Food engineering
  • Solar panels construction

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/cc
Water Absorption <= 0.010 %
@Time 346000 sec
DIN EN ISO 62
 <= 0.020 %
@Time 86400 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 129 MPaISO 2039-1
Tensile Strength 62.0 MPa50 mm/min; DIN EN ISO 527-2
Tensile Strength, Yield 62.0 MPa50 mm/min; DIN EN ISO 527-2
Elongation at Break 17 %50 mm/min; DIN EN ISO 527-2
Elongation at Yield 7.0 %50 mm/min; DIN EN ISO 527-2
Modulus of Elasticity 2.20 GPa
Flexural Strength 77.0 MPa
@Load 1.02 kg
2 mm/min; DIN EN ISO 178
Flexural Modulus 2.10 GPa
@Load 1.02 kg
2 mm/min; DIN EN ISO 178
Compressive Strength 16.0 MPa
@Strain 1 %,
Load 1.02 kg
5 mm/min; EN ISO 604
 28.0 MPa
@Strain 2 %,
Load 1.02 kg
5 mm/min; EN ISO 604
Compressive Modulus 1900 MPa
@Load 1.02 kg
5 mm/min; EN ISO 604
Charpy Impact Unnotched 150 kJ/m²Max. 7,5j; DIN EN ISO 179-1EU
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 160 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN EN ISO 11359-1;2
 180 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.30 J/g-°CISO 22007-4:2008
Thermal Conductivity 0.250 W/m-KISO 22007-4:2008
Melting Point 171 °CDIN 53765
Maximum Service Temperature, Air 150 °CShort term
 150 °CLong term
Glass Transition Temp, Tg -40.0 °CDIN 53765
Flammability, UL94 V-0DIN IEC 60995-11-10
 
Descriptive Properties
ColorWhite opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAID934 / 318895

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.