System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Americhem Engineered Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
V-0 rated polycarbonate-ABS alloy, excellent toughness and light stability
All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.
Key Words:
PC, ABS
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.19
g/cc
1.19
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
0.125 in.; ASTM D955
Melt Flow
14
g/10 min
@Load 2.16 kg,
Temperature 260 °C
14
g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
122
122
ASTM D785
Tensile Strength at Break
55.8
MPa
8100
psi
2.0 in/min; ASTM D638
Tensile Strength, Yield
60.0
MPa
8700
psi
2.0 in/min; ASTM D638
Elongation at Break
90 %
90 %
2.0 in/min; ASTM D638
Elongation at Yield
4.0 %
4.0 %
2.0 in/min; ASTM D638
Flexural Strength
95.1
MPa
13800
psi
2.0 in/min; ASTM D790
Flexural Modulus
2.70
GPa
392
ksi
2.0 in/min; ASTM D790
Izod Impact, Notched
6.41
J/cm
@Temperature 22.8 °C
12.0
ft-lb/in
@Temperature 73.0 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
95.0
°C
203
°F
Unannealed (0.250"); ASTM D648
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
210
-
254
°C
410
-
490
°F
Middle Barrel Temperature
216
-
260
°C
420
-
500
°F
Front Barrel Temperature
227
-
274
°C
440
-
525
°F
Nozzle Temperature
232
-
274
°C
450
-
525
°F
Melt Temperature
232
-
274
°C
450
-
525
°F
Mold Temperature
60.0
-
82.2
°C
140
-
180
°F
Drying Temperature
82.2
°C
180
°F
Dry Time
3
-
4
hour
3
-
4
hour
nominal; maximum drying time of 8 hours
Back Pressure
0.345
-
0.689
MPa
50.0
-
100
psi
Shot Size
30 - 60 %
30 - 60 %
Vent Depth
0.00381
-
0.00762
cm
0.00150
-
0.00300
in
Screw Speed
30
-
75
rpm
30
-
75
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
RTP Company RTP 2500 FR-110 Polycarbonate/ABS Alloy (PC/ABS), Flame Retardant - Halogen Free - UL94 V-0
Lotte Advanced Materials Infino® NH-1015S PC/ABS
Lotte Advanced Materials Infino® LM-1090 PC/ABS
PLTLC020 / 104405
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.