MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2500 FR-110 Polycarbonate/ABS Alloy (PC/ABS), Flame Retardant - Halogen Free - UL94 V-0
Categories: Polymer; Thermoplastic; ABS Polymer

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Water Absorption 0.15 %0.15 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.17 mm
0.0040 - 0.0060 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 35 - 50 g/10 min
@Load 5.00 kg,
Temperature 250 °C
35 - 50 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D 785
Tensile Strength at Break 55.2 MPa8000 psiASTM D 638
Elongation at Break >= 80 %>= 80 %ASTM D 638
Tensile Modulus 2.55 GPa370 ksiASTM D 638
Flexural Strength 86.2 MPa12500 psiASTM D 790
Flexural Modulus 2.76 GPa400 ksiASTM D 790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 21.4 J/cm
@Thickness 3.17 mm
40.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C205 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C190 °FASTM D 648
Flammability, UL94  V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 5VB
@Thickness 1.59 mm
5VB
@Thickness 0.0625 in
Oxygen Index 30 %30 %ASTM D 2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 274 °C470 - 525 °F
Mold Temperature 51.7 - 93.3 °C125 - 200 °F
Drying Temperature 93.3 °C200 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
RTP Company RTP 2599 X 67122 Polycarbonate/ABS Alloy (PC/ABS), Unreinforced - Flame Retardant - Halogen Free - UL94 V-0
Trinseo EMERGE™ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant

PQZWA757 / 92307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.