MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

European Black Locust Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Key Words: Robinia pseudoacacia; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.490 g/cc0.0177 lb/in³Earlywood
 0.680 g/cc0.0246 lb/in³Latewood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 7500 N1690 lb (f)Side
Tensile Strength, Ultimate 4.20 MPa609 psiPerpendicular to Grain
 133 MPa19300 psiAxial
Modulus of Rupture 0.102 GPa14.8 ksiStatic Bending
Flexural Modulus 11.07 GPa1606 ksiStatic Bending
Compressive Strength 18.6 MPa2700 psiPerpendicular to Grain
 70.0 MPa10200 psiParallel to Grain
Shear Strength 12.5 MPa1810 psiOrientation Unknown
Toughness 26.4 J19.5 ft-lb2 cm x 2 cm sample
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.10 %0.10 %Axial; Green to Zero Moisture
 4.0 %4.0 %Radial; Green to Zero Moisture
 6.5 %6.5 %Tangential; Green to Zero Moisture
 10.8 %10.8 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Black Locust Wood
European Birch Wood
Bigleaf Maple Wood
European Ash Wood
European Field Elm Wood

PTSE050 / 71314

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.