MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

European Ash Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Selected stock may be tough and be suitable for bending. Ring-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium/coarse
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Resistance to penetration by preservatives: Moderately Resistant
Common Applications: Interior joinery, sports goods

Key Words: Fraxinus excelsior; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.380 - 0.510 g/cc0.0137 - 0.0184 lb/in³Earlywood
 0.720 - 0.800 g/cc0.0260 - 0.0289 lb/in³Latewood
Cell Length 0.800 mm0.0315 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 6100 N1370 lb (f)Side
Tensile Strength, Ultimate 6.90 MPa1000 psiPerpendicular to Grain
 161 MPa23400 psiAxial
Modulus of Rupture 0.118 GPa17.1 ksiStatic Bending
Flexural Modulus 13.13 GPa1904 ksiStatic Bending
Compressive Strength 10.8 MPa1570 psiPerpendicular to Grain
 51.0 MPa7400 psiParallel to Grain
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 12.5 MPa1810 psiOrientation Unknown
Toughness 26.8 J19.8 ft-lb2 cm x 2 cm sample
Cleavage 6.90 kN/m39.4 lb/in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.20 %0.20 %Axial; Green to Zero Moisture
 5.2 %5.2 %Radial; Green to Zero Moisture
 8.3 %8.3 %Tangential; Green to Zero Moisture
 14 %14 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorWhite to light brown Usual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KT800-2X2T-200
American White Ash Wood
American Maple, Rock (Sugar Maple)
European Field Elm Wood
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-M46J-Plain Weave-280 GSM

PTSE010 / 71310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.