3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be readily applied with a spatula or extrusion gun. It will cure to a fuel-resistant rubber at temperatures above -6.7°C. It exhibits excellent tooling properties.Information provided by 3M |