Physical Properties | Metric | English | Comments |
---|
Density | 1.61 g/cc | 0.0582 lb/in³ |
Volatiles | <= 11 % | <= 11 % |
Brookfield Viscosity | 100000 - 400000 cP | 100000 - 400000 cP |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 40 | 40 |
| 55 | 55 |
Tensile Strength at Break | 2.07 MPa @Time 1.21e+6 sec | 300 psi @Time 336 hour |
| 1.52 MPa @Treatment Temp. 60.0 °C, Time 1.21e+6 sec | 220 psi @Treatment Temp. 140 °F, Time 336 hour |
| 2.14 MPa @Treatment Temp. 121 °C, Time 605000 sec | 310 psi @Treatment Temp. 250 °F, Time 168 hour |
Elongation at Break | 220 % @Time 1.21e+6 sec | 220 % @Time 336 hour |
| 180 % @Treatment Temp. 121 °C, Time 605000 sec | 180 % @Treatment Temp. 250 °F, Time 168 hour |
| 225 % @Treatment Temp. 60.0 °C, Time 1.21e+6 sec | 225 % @Treatment Temp. 140 °F, Time 336 hour |
Peel Strength | 3.68 kN/m @Temperature 60.0 °C, Time 605000 sec | 21.0 pli @Temperature 140 °F, Time 168 hour |
| 3.68 kN/m @Temperature 60.0 °C, Time 605000 sec | 21.0 pli @Temperature 140 °F, Time 168 hour |
| 4.21 kN/m @Temperature 60.0 °C, Time 605000 sec | 24.0 pli @Temperature 140 °F, Time 168 hour |
| 4.21 kN/m @Temperature 60.0 °C, Time 605000 sec | 24.0 pli @Temperature 140 °F, Time 168 hour |
| 4.38 kN/m @Temperature 60.0 °C, Time 605000 sec | 25.0 pli @Temperature 140 °F, Time 168 hour |
| 4.38 kN/m @Temperature 60.0 °C, Time 605000 sec | 25.0 pli @Temperature 140 °F, Time 168 hour |
| 4.38 kN/m @Temperature 60.0 °C, Time 605000 sec | 25.0 pli @Temperature 140 °F, Time 168 hour |
| 4.56 kN/m @Temperature 60.0 °C, Time 605000 sec | 26.0 pli @Temperature 140 °F, Time 168 hour |
| 4.56 kN/m @Temperature 60.0 °C, Time 605000 sec | 26.0 pli @Temperature 140 °F, Time 168 hour |
| 4.73 kN/m @Temperature 60.0 °C, Time 605000 sec | 27.0 pli @Temperature 140 °F, Time 168 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Maximum Service Temperature, Air | 121 °C | 250 °F |
Minimum Service Temperature, Air | -54.0 °C | -65.2 °F |
|
Processing Properties | Metric | English | Comments |
---|
Cure Time | 120 min @Temperature 25.0 °C | 2.00 hour @Temperature 77.0 °F |
| 480 min @Temperature 4.40 °C | 8.00 hour @Temperature 39.9 °F |
| 840 min @Temperature -6.70 °C | 14.0 hour @Temperature 19.9 °F |
Tack-Free Time | 70.2 min @Temperature 25.0 °C | 1.17 hour @Temperature 77.0 °F |
| 420 min @Temperature 4.40 °C | 7.00 hour @Temperature 39.9 °F |
| 720 min @Temperature -6.70 °C | 12.0 hour @Temperature 19.9 °F |
Shelf Life | 6.00 Month @Temperature <=26.7 °C | 6.00 Month @Temperature <=80.1 °F |
|
Descriptive Properties |
---|
Alkalinity | 13 |
Appearance | Dark Brown |
| Gray |
| White |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.