MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M AC-250 A-1/6 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable liquid which can be applied with a spatula, extrusion gun, roller, or brush. It will cure to a fuel-resistant rubber at temperatures above -6.7°C.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccAMS-S83318
Volatiles <= 11 %
Brookfield Viscosity 100000 - 400000 cPBase, RVF #6 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40Hydrolytic Stability; AMS-S83318
 55AMS-S83318
Tensile Strength at Break 2.07 MPa
@Time 1.21e+6 sec
Standard Cure; AMS-S83318
 1.52 MPa
@Treatment Temp. 60.0 °C,
Time 1.21e+6 sec
JRF; AMS-S83318
 2.14 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
JRF; AMS-S83318
Elongation at Break 220 %
@Time 1.21e+6 sec
Standard Cure; AMS-S83318
 180 %
@Treatment Temp. 121 °C,
Time 605000 sec
JRF; AMS-S83318
 225 %
@Treatment Temp. 60.0 °C,
Time 1.21e+6 sec
JRF; AMS-S83318
Peel Strength 21.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Stainless Steel; AMS-S83318
 21.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Alodine; AMS-S83318
 24.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, MIL-C-27725; AMS-S83318
 24.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Alclad; AMS-S83318
 25.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, MIL-C-27725; AMS-S83318
 25.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Alclad; AMS-S83318
 25.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Titanium; AMS-S83318
 26.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Stainless Steel; AMS-S83318
 26.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF, Alodine; AMS-S83318
 27.0 pli
@Temperature 60.0 °C,
Time 605000 sec
JRF/SW, Titanium; AMS-S83318
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CAMS-S83318
Minimum Service Temperature, Air -54.0 °CAMS-S83318
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 25.0 °C
 8.00 hour
@Temperature 4.40 °C
 14.0 hour
@Temperature -6.70 °C
Tack-Free Time 1.17 hour
@Temperature 25.0 °C
 7.00 hour
@Temperature 4.40 °C
 12.0 hour
@Temperature -6.70 °C
Shelf Life 6.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
Alkalinity13
AppearanceDark BrownAccelerator
 Gray
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Master Bond EP21TPLV Two Component Epoxy System
Master Bond EP21TPND Two Component Polysulfide Epoxy Adhesive
Abatron AboSeal 8104-11 Polysulfide, Thixotropic Sealant and Caulk
Abatron AboSeal 8104-10 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk

PMM35412 / 170159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.