Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of densities and sizes. Kaowool blanket offers excellent handleability and high temperature stability. This allows it to meet a wide range of hot face and backup insulation applications in furnaces, kilns and other equipment requiring high temperature heat containment. Military Specifications and Approvals: Mil-I-23128A- 3, 6 pcf blanketMil-I-24244- all blanketsMil-I-23128B- 6, 8 pcf blanketInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |