MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber
Categories: Ceramic; Oxide

Material Notes: Ceramic fiber Papers are manufactured from high purity refractory fibers and designed for high temperature insulation. Advanced production techniques ensure uniform fiber distribution and close control of thickness and density. Papers are being produced from Alumina silicate fibers with minimum addition of carefully selected Bonds, which burn out cleanly in service.

Applications:

  • Insulating gaskets
  • Expansion joints
  • Die cut gaskets for domestic appliances
  • Gaskets, seals & parting media
  • Ladle lining back up
  • Mould liners
  • Thermal barrier for vehicles(Silencers,catalytic exhaust and heat shields)
  • Parting media
  • Heat loss reduction in sub entry nozzle

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.150 g/cc0.00542 lb/in³nominal
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 883 MPa128000 psiENV-1094-7
 
Thermal PropertiesMetricEnglishComments
Shrinkage <= 2.0 %
@Temperature 1100 °C,
Time 86400 sec
<= 2.0 %
@Temperature 2010 °F,
Time 24.0 hour
ENV-1094-7
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 42 %>= 42 %
Loss on Ignition(%) <= 10 %<= 10 %
SiO2 <= 56 %<= 56 %
 
Descriptive Properties
Classification Temperature (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel CA15C
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
ExxonMobil C6LL 1017.32 Cast Linear Low Density Polyethylene Resin
Hardwire 3x2-4-12 Low Density Tape
Morgan Advanced Ceramics Cerachrome™ Blanket Thermal Ceramic

CMORF7025 / 203324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.