MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MOCOM (ALBIS) Tedur® P 9519 PPS, ~45% Glass Fiber (black only)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.

Applications: Handles, Fixing Elements

Processing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccDIN 53 47
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaDIN 53 455
Elongation at Break 1.6 %DIN 53 455
Modulus of Elasticity 16.0 GPaDIN 53 457
Flexural Yield Strength 240 MPaDIN 53 452
Flexural Modulus 14.0 GPaDIN 53 457
Izod Impact, Notched 2.99 J/cmApproximation; ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °CASTM D648
Flammability, UL94 V-0Albis Internal Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 321 - 341 °CInjection
Mold Temperature 141 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MOCOM (ALBIS) Tedur® L 9523 PPS, 60% Glass Fiber/Mineral
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead

PA1D45 / 21940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.