Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form identified: Kraton G7705 GI-N - supplied as a dense, natural color pelletRegion: North America; Asia Pacific; Europe; Japan; and South America Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Bitumen Modification; Footwear; and Impact Modification Information provided by Kraton® |