MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G2705 GU (SEBS) Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good puncture resealing characteristics. It is also steam sterilizable. It is supplied from North America in the physical form identified:
G2705 GU-N - supplied as a transparent pellet.

Region: Asia Pacific, Europe, Japan, North America, and South America

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.875 - 0.905 g/cc0.875 - 0.905 g/ccBAM 1014
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 52 - 6252 - 62Injection molded plaque at 205°C; BAM 1003
Tensile Strength 5.79 MPa840 psiInjection molded plaques, Die C, Machine Direction; ASTM D412
 11.38 MPa1651 psiInjection molded plaques, Die C, Cross Direction; ASTM D412
Elongation at Break 650 %650 %Injection molded plaques, Die C, Machine Direction; ASTM D412
Elongation at Yield >= 800 %>= 800 %Injection molded plaques, Die C, Cross Direction; ASTM D412
100% Modulus  1.62 MPa
@Strain 100 %
235 psi
@Strain 100 %
Injection molded plaques, Die C, Cross Direction; ASTM D412
 1.93 MPa
@Strain 100 %
280 psi
@Strain 100 %
Injection molded plaques, Die C, Machine Direction; ASTM D412
300% Modulus  2.52 MPa
@Strain 300 %
366 psi
@Strain 300 %
Injection molded plaques, Die C, Cross Direction; ASTM D412
 2.89 MPa
@Strain 300 %
419 psi
@Strain 300 %
Injection molded plaques, Die C, Machine Direction; ASTM D412
Tear Strength 27.2 kN/m155 pliInjection molded plaques, Die C, Machine Direction; ASTM D624
 29.8 kN/m170 pliInjection molded plaques, Die C, Cross Direction; ASTM D624
Compression Set 19 %
@Temperature 23.0 °C,
Time 79200 sec
19 %
@Temperature 73.4 °F,
Time 22.0 hour
Injection molded plaque; ASTM D395B
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® G2708 GU (SEBS) Compound
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G7705 GI-B (SEBS) Compound
Kraton® G7705 GI-N (SEBS) Compound

PKRA9908 / 132807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.