MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).

Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.

Uses: Injection molding.

Availability: Americas and Asia

Information Provided by The Lubrizol Corporation

Key Words: RETPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.00070 cm/cm0.00070 in/inflex bar; ASTM D955
 0.0020 cm/cm0.0020 in/indisc; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 61
@Time 5.00 sec
55 - 61
@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 28.0 MPa4060 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Tensile Modulus 0.620 GPa89.9 ksiASTM D638
Flexural Strength 19.0 MPa2760 psiASTM D790
Flexural Modulus 0.570 GPa82.7 ksiASTM D790
Izod Impact, Notched  0.850 J/cm
@Temperature -40.0 °C
1.59 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 6.40 J/cm
@Temperature 23.0 °C
12.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C124 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 213 °C415 °F
Middle Barrel Temperature 218 °C424 °F
Front Barrel Temperature 218 °C424 °F
Nozzle Temperature 221 °C430 °F
Melt Temperature 227 °C441 °F
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
Injection Pressure 69.0 - 103 MPa10000 - 14900 psi
Hold Pressure 35.0 - 69.0 MPa5080 - 10000 psi
Back Pressure 0.345 MPa50.0 psi
Screw Speed 30 - 80 rpm30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlthane® MB-51UV Thermoplastic Polyurethane Elastomer

PNOVEON501 / 121392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.