MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax SG802N Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Pro-fax SG802N high impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers very good cold temperature impact resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax SG802N.

Availability: North America

Application: Interior Automotive Applications; TWIM Food Containers; Underhood

Market: Automotive; Rigid Packaging

Processing Method: Compounding; Injection Molding

Attribute: Low Temperature Impact Resistance; Nucleated

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccMethod A; ISO 1183-1
Melt Flow 35.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.0 MPaISO 527-1, -2
Elongation at Yield 5.00 %ISO 527-1, -2
Flexural Modulus 1120 MPaISO 178
Izod Impact, Notched (ISO) 5.30 kJ/m²
@Temperature -40.0 °C
ISO 180
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact, Notched 4.50 kJ/m²
@Temperature -40.0 °C
ISO 179
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CUnannealed; ISO 75A-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9779 / 324714

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.