Pro-fax SG802N high impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers very good cold temperature impact resistance. ASTM and ISO-based versions of the technical data sheet are available for Pro-fax SG802N. Availability: North America Application: Interior Automotive Applications; TWIM Food Containers; Underhood Market: Automotive; Rigid Packaging Processing Method: Compounding; Injection Molding Attribute: Low Temperature Impact Resistance; Nucleated Information provided by LyondellBasell. |