MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CIMBAR Suspengel™ 200 High Purity Bentonite, Industrial Grade
Categories: Ceramic; Clay; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process control assures our customers of the most consistent products on the market.

Typical Industrial Uses:

  • Agricultural Products - Pesticides, Fertilizers, Fungicides
  • Coatings Market - Rheological additive, Suspension
  • Paper Industry - Suspension, De-Inking
  • Industrial Markets - Ceramics, Adhesives, Caulks, Sealants, Foundry/Refractory
  • Environmental Applications - Water Treatment, Waste Treatment, Pond/Lake Sealing
<

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/cc
Bulk Density 1.15 g/cc0.0417 lb/in³
Oil Absorption 38 %38 %g oil/100 g filler; ASTM D281-31
Moisture Absorption at Equilibrium 8.0 %8.0 %
Loss On Ignition 11 %11 %
Particle Mesh Size 200 Mesh200 Mesh80.0% passing, dry
 200 Mesh200 Mesh98.0% passing, wet
 325 Mesh325 Mesh95.0% passing, wet
pH 9.09.0
Viscosity 9.5 cP9.5 cPApparent
Viscosity Measurement 9.09.0Plastic Viscosity (FV)
 
Component Elements PropertiesMetricEnglishComments
Al2O3 21.4 %21.4 %
CaO <= 0.70 %<= 0.70 %
Fe2O3 3.8 %3.8 %
K2O 0.30 %0.30 %
MgO 2.0 %2.0 %
Na2O 2.7 %2.7 %
SiO2 63.3 %63.3 %
 
Descriptive Properties
Base Exchange Capacity (meq/kg)1050
Surface Area N2 Absorption (m²/g)20
Yield Point (Lb/100 ft²)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Overview of materials for Polyetheretherketone, Unreinforced
Montmorillonite Al2O3-4SiO2-nH2O
Kaolinite (Al2O3-2SiO2-2H2O)
Illite KAl2(AlSi3O10)-(OH)2

CIMBAR959 / 133441

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.