MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 8600-20 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 8600 is a translucent, ignition-resistant and easy flow polycarbonate resin. This resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental standards. It has a UL94 flammability rating of V-0 at 1.5 mm.

Applications:

  • A broad range of injection molded applications in the electronics, electrical and information technology equipment markets

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/B
Linear Mold Shrinkage 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 123ISO 2039-2
Tensile Strength at Break 58.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Elongation at Break 100 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Elongation at Yield 6.0 %
@Thickness 4.00 mm
Injection Molded; ISO 527-2/50
Flexural Strength 94.0 MPa
@Thickness 4.00 mm
Injection Molded, 2.0 mm/min; ISO 178
Flexural Modulus 2400 MPaInjection Molded, 2.0 mm/min; ISO 178
Izod Impact, Notched 690 J/mInjection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ISO 11359-2
Hot Ball Pressure Test >= 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 136 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °CUnannealed; ISO 75-2/A
Vicat Softening Point 143 °CISO 306/B50
 150 °CISO 306/A120
UL RTI, Electrical 125 °CUL 746
UL RTI, Mechanical with Impact 125 °CUL 746
UL RTI, Mechanical without Impact 125 °CUL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
Oxygen Index 35 %ISO 4589-2
Glow Wire Ignition Temperature 960 °C
@Thickness 1.50 mm
IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 125 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 8600-10 Polycarbonate
Trinseo EMERGE™ PC 8702-15 (AP) Polycarbonate Resin
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Aclo Accucomp Polycarbonate POL051L Medium Viscosity
Evonik Vestodur® 2000 Medium Viscosity PBT

PDOW1370 / 30588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.