Physical Properties | Original Value | Comments |
---|
Density | 1.22 - 1.80 g/cc |
| 1.14 - 1.32 g/cc @Temperature 205 - 250 °C |
Filler Content | 15.0 - 20.0 % |
Water Absorption | 0.0100 - 0.500 % |
Moisture Absorption at Equilibrium | 0.0200 - 0.400 % |
Water Absorption at Saturation | 0.150 - 0.500 % |
Viscosity | 150000 cP |
| 17.0 - 18.0 cP @Temperature 250 - 265 °C |
| 17.0 - 18.0 cP @Load 5.00 - 5.00 kg |
| 9.00 - 460190 cP @Shear Rate 10.0 - 100000 1/s |
| 9.00 - 460190 cP @Temperature 230 - 280 °C |
Viscosity Test | 69.0 - 116 cm³/g |
Viscosity Number | 94.0 - 135 cm³/g |
Maximum Moisture Content | 0.0200 - 0.0400 |
| 0.200 - 0.200 @Temperature 120 - 120 °C |
| 0.200 - 0.200 @Time 299 - 299 sec |
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm |
| 0.00400 - 0.00400 cm/cm @Temperature 80.0 - 80.0 °C |
| 0.00300 - 0.00400 cm/cm @Temperature 260 - 260 °C |
| 0.00300 - 0.00400 cm/cm @Pressure 60.0 - 60.0 MPa |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0180 cm/cm |
| 0.0110 - 0.0120 cm/cm @Temperature 80.0 - 80.0 °C |
| 0.0100 - 0.0110 cm/cm @Temperature 260 - 260 °C |
| 0.0100 - 0.0110 cm/cm @Pressure 60.0 - 60.0 MPa |
Melt Flow | 2.00 - 58.0 g/10 min |
Spiral Flow | 36.0 - 43.0 cm |
Ash | 13.0 - 24.0 % |
| 15.0 - 15.0 % @Temperature 625 - 625 °C |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Rockwell M | 70.0 - 109 |
Hardness, Rockwell R | 90.0 - 120 |
Ball Indentation Hardness | 128 - 200 MPa |
Tensile Strength, Ultimate | 47.0 - 140 MPa |
| 40.0 - 165 MPa @Temperature -40.0 - 150 °C |
Tensile Strength, Yield | 62.1 - 125 MPa |
Elongation at Break | 1.00 - 155 % |
| 1.90 - 6.30 % @Temperature 0.000 - 150 °C |
Elongation at Yield | 2.00 - 115 % |
Modulus of Elasticity | 3.50 - 14.0 GPa |
| 2.06843 - 6.41212 GPa @Temperature -40.0 - 150 °C |
Flexural Yield Strength | 86.0 - 190 MPa |
| 80.0 - 80.0 MPa @Temperature 90.0 - 90.0 °C |
Flexural Modulus | 3.20 - 10.0 GPa |
| 3.50 - 5.00 GPa @Temperature 60.0 - 120 °C |
Flexural Strain at Break | 3.00 - 4.50 % |
Flexural Strain at Yield | 3.70 - 4.40 % |
Poissons Ratio | 0.340 - 0.370 |
Izod Impact | 50.0 J |
| 50.0 - 50.0 J @Temperature -30.0 - 0.000 °C |
Izod Impact, Notched | 0.267 - 1.60 J/cm |
| 0.430 - 0.600 J/cm @Temperature -40.0 - -20.0 °C |
Izod Impact, Unnotched | 0.588 - 8.17 J/cm |
| 3.30 - 3.60 J/cm @Temperature -30.0 - -30.0 °C |
Izod Impact, Notched (ISO) | 3.50 - 60.0 kJ/m² |
| 4.00 - 10.0 kJ/m² @Temperature -40.0 - 30.0 °C |
Izod Impact, Unnotched (ISO) | 12.2 - 65.0 kJ/m² |
| 10.5 - 55.0 kJ/m² @Temperature -40.0 - 30.0 °C |
Charpy Impact Unnotched | 0.450 - 6.90 J/cm² |
| 1.39 - 6.50 J/cm² @Temperature -40.0 - -20.0 °C |
Charpy Impact, Notched | 0.350 - 2.00 J/cm² |
| 0.300 - 1.00 J/cm² @Temperature -40.0 - -20.0 °C |
Dart Drop, Total Energy | 5.00 J |
Coefficient of Friction | 0.150 - 0.200 |
Tensile Creep Modulus, 1 hour | 3500 - 7300 MPa |
Tensile Creep Modulus, 1000 hours | 2400 - 6900 MPa |
|
Electrical Properties | Original Value | Comments |
---|
Electrical Resistivity | 1.00e+13 - 1.00e+17 ohm-cm |
Surface Resistance | 120 - 3.00e+17 ohm |
Dielectric Constant | 2.70 - 5.20 |
Dielectric Strength | 14.0 - 100 kV/mm |
Dissipation Factor | 0.000700 - 0.150 |
Dielectric Loss Index | 0.00200 - 0.0200 |
Arc Resistance | 0.000 - 180 sec |
Comparative Tracking Index | 125 - 600 V |
Hot Wire Ignition, HWI | 7.00 - 120 sec |
High Amp Arc Ignition, HAI | 30.0 - 120 arcs |
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 150 mm/min |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 20.0 - 110 µm/m-°C |
| 30.0 - 30.0 µm/m-°C @Temperature 50.0 - 120 °C |
CTE, linear, Transverse to Flow | 61.0 - 173 µm/m-°C |
| 150 - 150 µm/m-°C @Temperature 50.0 - 120 °C |
Specific Heat Capacity | 1.50 - 1.84 J/g-°C |
| 1.85 - 1.90 J/g-°C @Temperature 205 - 250 °C |
Thermal Conductivity | 0.150 - 0.280 W/m-K |
| 0.240 - 0.260 W/m-K @Temperature 205 - 250 °C |
Melting Point | 178 - 255 °C |
Maximum Service Temperature, Air | 75.0 - 330 °C |
Hot Ball Pressure Test | 125 - 215 °C |
Deflection Temperature at 0.46 MPa (66 psi) | 99.0 - 230 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 - 220 °C |
Deflection Temperature at 8.0 MPa | 65.0 - 140 °C |
Vicat Softening Point | 128 - 220 °C |
Glass Transition Temp, Tg | 44.0 - 65.0 °C |
UL RTI, Electrical | 50.0 - 140 °C |
UL RTI, Mechanical with Impact | 50.0 - 140 °C |
UL RTI, Mechanical without Impact | 50.0 - 140 °C |
Flammability, UL94 | HB - 5VA |
Flame Spread | 24.0 - 100 mm/min |
Oxygen Index | 19.0 - 35.0 % |
Glow Wire Test | 650 - 960 °C |
|
Processing Properties | Original Value | Comments |
---|
Processing Temperature | 20.0 - 275 °C |
Nozzle Temperature | 225 - 270 °C |
Die Temperature | 240 - 275 °C |
Melt Temperature | 203 - 280 °C |
Mold Temperature | 30.0 - 130 °C |
Injection Velocity | 70.0 - 300 mm/sec |
Drying Temperature | 80.0 - 140 °C |
Moisture Content | 0.000 - 0.400 % |
Dew Point | -40.0 - -28.9 °C |
Injection Pressure | 3.50 - 120 MPa |
Vent Depth | 0.00127 - 0.00381 cm |
Hot-Working Temperature | 250 - 260 °C |
Precipitation Temperature | 40.0 - 60.0 °C |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.