Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.14 g/cc | 1.14 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 79 | 79 |
| 55 @Treatment Temp. 23.0 °C, Time 252000 sec | 55 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 71 @Treatment Temp. 100 °C, Time 252000 sec | 71 @Treatment Temp. 212 °F, Time 70.0 hour |
| 74 @Treatment Temp. 100 °C, Time 252000 sec | 74 @Treatment Temp. 212 °F, Time 70.0 hour |
| 76 @Treatment Temp. 23.0 °C, Time 252000 sec | 76 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 82 @Treatment Temp. 100 °C, Time 252000 sec | 82 @Treatment Temp. 212 °F, Time 70.0 hour |
| 88 @Treatment Temp. 100 °C, Time 252000 sec | 88 @Treatment Temp. 212 °F, Time 70.0 hour |
| 91 @Treatment Temp. 125 °C, Time 252000 sec | 91 @Treatment Temp. 257 °F, Time 70.0 hour |
Tensile Strength | 21.60 MPa | 3133 psi |
| 7.6249 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1105.9 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 17.20 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 2494 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 19.441 MPa @Treatment Temp. 100 °C, Time 252000 sec | 2819.7 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 20.262 MPa @Treatment Temp. 125 °C, Time 252000 sec | 2938.8 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 21.904 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3176.9 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 22.889 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3319.8 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 25.576 MPa @Treatment Temp. 100 °C, Time 252000 sec | 3709.5 psi @Treatment Temp. 212 °F, Time 70.0 hour |
Elongation, Ultimate | 400 % | 400 % |
| 196 % @Treatment Temp. 125 °C, Time 252000 sec | 196 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 234 % @Treatment Temp. 23.0 °C, Time 252000 sec | 234 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 338 % @Treatment Temp. 100 °C, Time 252000 sec | 338 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 350 % @Treatment Temp. 100 °C, Time 252000 sec | 350 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 362.8 % @Treatment Temp. 100 °C, Time 252000 sec | 362.8 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 366.8 % @Treatment Temp. 100 °C, Time 252000 sec | 366.8 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 370.8 % @Treatment Temp. 23.0 °C, Time 252000 sec | 370.8 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
100% Modulus | 4.43 MPa | 643 psi |
Tear Strength | 50.8 kN/m | 290 pli |
Compression Set | 22.4 % @Treatment Temp. 100 °C, Time 79200 sec | 22.4 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 30 % @Treatment Temp. 100 °C, Time 79200 sec | 30 % @Treatment Temp. 212 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -47.8 °C | -54.0 °F |
Shrinkage | -4.40 % @Treatment Temp. 100 °C, Time 252000 sec | -4.40 % @Treatment Temp. 212 °F, Time 70.0 hour |
| -4.30 % @Treatment Temp. 125 °C, Time 252000 sec | -4.30 % @Treatment Temp. 257 °F, Time 70.0 hour |
| -2.40 % @Treatment Temp. 100 °C, Time 252000 sec | -2.40 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 4.4 % @Treatment Temp. 23.0 °C, Time 252000 sec | 4.4 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 7.1 % @Treatment Temp. 100 °C, Time 252000 sec | 7.1 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 13.1 % @Treatment Temp. 100 °C, Time 252000 sec | 13.1 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 41.9 % @Treatment Temp. 23.0 °C, Time 252000 sec | 41.9 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |