Compound 77757 is a 75 durometer black colored Carboxylated Nitrile elastomer, it is formulated with an organic lubricant to provide internal lubrication. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 820 B14 EO14 EO34 Z1; 3 BG 830 B14 EO14 Z1; 4 BG 830 B14 EO14 Z1; 6 BG 820 A14 B14 EO14 EO34 F17 Z1; 7 BG 820 B14 EO14 EO34 EF11 F16 EA14 Z1 Z1 = 75 +/- 5 SHORE A Information provided by Pressure Seals Inc. |