MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Texin® RxS285 Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: Texin RxS285 resin is an aromatic polyester-based thermoplastic polyurethane. It can be processed by injection molding, extrusion or blow molding.

Properties / Applications: Texin RxS285 offers outstanding abrasion resistance, impact strength, toughness and flexibility. Typical medical applications include dental ligature, tubing and luers. As with any product, the use of Texin RxS285 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.202 g/cc1.202 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Melt Flow 4.0 g/10 min
@Load 8.70 kg,
Temperature 190 °C
4.0 g/10 min
@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength at Break 37.9 MPa5500 psiASTM D412
Tensile Stress at Strain  5.34 MPa
@Strain 100 %
775 psi
@Strain 100 %
ASTM D412
 13.1 MPa
@Strain 300 %
1900 psi
@Strain 300 %
ASTM D412
Elongation at Break 500 %500 %ASTM D412
Flexural Modulus 0.0276 GPa4.00 ksiASTM D790
Tear Strength 87.6 kN/m500 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 35
@Load 1.00 kg
35
@Load 2.20 lb
[mg] Loss, H-18; ASTM D3489
Compression Set  12 %
@Temperature 23.0 °C,
Time 79200 sec
12 %
@Temperature 73.4 °F,
Time 22.0 hour
postcured; ASTM D395-B
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
postcured; ASTM D395-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 91.0 °C196 °FRate A; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Yellow Index <= 15 %<= 15 %ASTM E313
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 199 °C360 - 390 °FInjection
 182 - 199 °C360 - 390 °FExtrusion
Middle Barrel Temperature 182 - 204 °C360 - 399 °FInjection
 182 - 204 °C360 - 399 °FExtrusion
Front Barrel Temperature 182 - 210 °C360 - 410 °FInjection
 182 - 210 °C360 - 410 °FExtrusion
Nozzle Temperature 188 - 213 °C370 - 415 °FInjection
Die Temperature 188 - 210 °C370 - 410 °FExtrusion
Melt Temperature 191 - 204 °C376 - 399 °FExtrusion
 196 - 207 °C385 - 405 °FInjection
Mold Temperature 16.0 - 43.0 °C60.8 - 109 °FInjection
Injection Pressure 41.4 - 103 MPa6000 - 15000 psiInjection
Back Pressure <= 5.52 MPa<= 800 psiInjection
Cushion <= 0.317 cm<= 0.125 inInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® RxT90A Thermoplastic Polyurethanes (TPU)
Covestro Texin® RxT85A Thermoplastic Polyurethanes (TPU)
LG Chemical LG-485 Styrene-Butadiene-Styrene
Dynasol Calprene® 485 Thermoplastic Rubber SBS Oil extended
Covestro Texin® STX Thermoplastic Polyurethanes (TPU)

PCOVEST0994 / 202777

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.