MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LG-485 Styrene-Butadiene-Styrene  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Radial structure, Oil Extended Grade Thermoplastic Elastomer

Applications: Compounding Plastic Modifier

CAS: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccISO 2781
Volatiles <= 0.50 %<= 0.50 %ASTM D1416
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
13 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Chemical PropertiesMetricEnglishComments
Styrene Content 32 %32 %LSYQBSD015
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5151ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Flash Point 288 °C550 °F
 
Descriptive Properties
Oil Contents45 phrASTM D1416

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dynasol Calprene® 485 Thermoplastic Rubber SBS Oil extended
Celanese SO.F.TER Sofprene T® 5420.A85 SBS TPE
Celanese SO.F.TER Sofprene T® 5402.A85 SBS TPE
Overview of materials for Styrene/Butadiene/Styrene (SBS)
RTP Company RTP 2740U-80A  Saturated Styrenic Elastomer (SBS) 80 Shore A

PLAY397 / 148407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.