Physical Properties | Metric | English | Comments |
---|
Density | 7.80 g/cc | 0.282 lb/in³ |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Brinell | 237 @Temperature 705 °C | 237 @Temperature 1300 °F |
| 253 @Temperature 650 °C | 253 @Temperature 1200 °F |
| 266 @Temperature 595 °C | 266 @Temperature 1100 °F |
| 318 @Temperature 540 °C | 318 @Temperature 1000 °F |
| 360 @Temperature 260 °C | 360 @Temperature 500 °F |
| 360 @Temperature 370 °C | 360 @Temperature 698 °F |
| 360 @Temperature 480 °C | 360 @Temperature 896 °F |
| 365 @Temperature 150 °C | 365 @Temperature 302 °F |
Hardness, Knoop | 250 @Temperature 705 °C | 250 @Temperature 1300 °F |
| 268 @Temperature 650 °C | 268 @Temperature 1200 °F |
| 283 @Temperature 595 °C | 283 @Temperature 1100 °F |
| 343 @Temperature 540 °C | 343 @Temperature 1000 °F |
| 392 @Temperature 260 °C | 392 @Temperature 500 °F |
| 392 @Temperature 370 °C | 392 @Temperature 698 °F |
| 392 @Temperature 480 °C | 392 @Temperature 896 °F |
| 397 @Temperature 150 °C | 397 @Temperature 302 °F |
Hardness, Rockwell C | 20 @Temperature 705 °C | 20 @Temperature 1300 °F |
| 23.5 @Temperature 650 °C | 23.5 @Temperature 1200 °F |
| 26 @Temperature 595 °C | 26 @Temperature 1100 °F |
| 34 @Temperature 540 °C | 34 @Temperature 1000 °F |
| 39 @Temperature 260 °C | 39 @Temperature 500 °F |
| 39 @Temperature 370 °C | 39 @Temperature 698 °F |
| 39 @Temperature 480 °C | 39 @Temperature 896 °F |
| 39.5 @Temperature 150 °C | 39.5 @Temperature 302 °F |
Hardness, Vickers | 242 @Temperature 705 °C | 242 @Temperature 1300 °F |
| 260 @Temperature 650 °C | 260 @Temperature 1200 °F |
| 275 @Temperature 595 °C | 275 @Temperature 1100 °F |
| 332 @Temperature 540 °C | 332 @Temperature 1000 °F |
| 378 @Temperature 260 °C | 378 @Temperature 500 °F |
| 378 @Temperature 370 °C | 378 @Temperature 698 °F |
| 378 @Temperature 480 °C | 378 @Temperature 896 °F |
| 383 @Temperature 150 °C | 383 @Temperature 302 °F |
Tensile Strength, Ultimate | 741 MPa @Temperature 705 °C | 107000 psi @Temperature 1300 °F |
| 796 MPa @Temperature 650 °C | 115000 psi @Temperature 1200 °F |
| 865 MPa @Temperature 595 °C | 125000 psi @Temperature 1100 °F |
| 1080 MPa @Temperature 540 °C | 157000 psi @Temperature 1000 °F |
| 1185 MPa @Temperature 480 °C | 171900 psi @Temperature 896 °F |
| 1260 MPa @Temperature 370 °C | 183000 psi @Temperature 698 °F |
| 1295 MPa @Temperature 260 °C | 187800 psi @Temperature 500 °F |
| 1310 MPa @Temperature 150 °C | 190000 psi @Temperature 302 °F |
Tensile Strength, Yield | 600 MPa @Strain 0.2 %, Temperature 705 °C | 87000 psi @Strain 0.2 %, Temperature 1300 °F |
| 670 MPa @Strain 0.2 %, Temperature 650 °C | 97200 psi @Strain 0.2 %, Temperature 1200 °F |
| 740 MPa @Strain 0.2 %, Temperature 595 °C | 107000 psi @Strain 0.2 %, Temperature 1100 °F |
| 895 MPa @Strain 0.2 %, Temperature 540 °C | 130000 psi @Strain 0.2 %, Temperature 1000 °F |
| 962 MPa @Strain 0.2 %, Temperature 150 °C | 140000 psi @Strain 0.2 %, Temperature 302 °F |
| 962 MPa @Strain 0.2 %, Temperature 260 °C | 140000 psi @Strain 0.2 %, Temperature 500 °F |
| 962 MPa @Strain 0.2 %, Temperature 370 °C | 140000 psi @Strain 0.2 %, Temperature 698 °F |
| 983 MPa @Strain 0.2 %, Temperature 480 °C | 143000 psi @Strain 0.2 %, Temperature 896 °F |
Elongation at Break | 9.0 % @Temperature 150 °C | 9.0 % @Temperature 302 °F |
| 9.5 % @Temperature 260 °C | 9.5 % @Temperature 500 °F |
| 13 % @Temperature 540 °C | 13 % @Temperature 1000 °F |
| 14 % @Temperature 370 °C | 14 % @Temperature 698 °F |
| 16 % @Temperature 480 °C | 16 % @Temperature 896 °F |
| 17 % @Temperature 595 °C | 17 % @Temperature 1100 °F |
| 17.5 % @Temperature 650 °C | 17.5 % @Temperature 1200 °F |
| 20 % @Temperature 705 °C | 20 % @Temperature 1300 °F |
Modulus of Elasticity | 200 GPa | 29000 ksi |
Poissons Ratio | 0.20 | 0.20 |
Shear Modulus | 83.0 GPa | 12000 ksi |
Izod Impact | 20.3 J @Temperature 150 °C | 15.0 ft-lb @Temperature 302 °F |
| 20.3 J @Temperature 260 °C | 15.0 ft-lb @Temperature 500 °F |
| 20.3 J @Temperature 370 °C | 15.0 ft-lb @Temperature 698 °F |
| 20.3 J @Temperature 480 °C | 15.0 ft-lb @Temperature 896 °F |
| 27.3 J @Temperature 540 °C | 20.1 ft-lb @Temperature 1000 °F |
| 54.4 J @Temperature 595 °C | 40.1 ft-lb @Temperature 1100 °F |
| 61.1 J @Temperature 650 °C | 45.1 ft-lb @Temperature 1200 °F |
| 75.0 J @Temperature 705 °C | 55.3 ft-lb @Temperature 1300 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Electrical Resistivity | 0.0000570 ohm-cm @Temperature 20.0 °C | 0.0000570 ohm-cm @Temperature 68.0 °F |
| 0.000108 ohm-cm @Temperature 650 °C | 0.000108 ohm-cm @Temperature 1200 °F |
Magnetic Permeability | 700 - 1000 | 700 - 1000 |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 9.90 µm/m-°C @Temperature 0.000 - 100 °C | 5.50 µin/in-°F @Temperature 32.0 - 212 °F |
| 11.0 µm/m-°C @Temperature 0.000 - 315 °C | 6.11 µin/in-°F @Temperature 32.0 - 599 °F |
| 11.5 µm/m-°C @Temperature 0.000 - 540 °C | 6.39 µin/in-°F @Temperature 32.0 - 1000 °F |
| 11.7 µm/m-°C @Temperature 0.000 - 650 °C | 6.50 µin/in-°F @Temperature 32.0 - 1200 °F |
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C | 0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
Thermal Conductivity | 24.9 W/m-K @Temperature 100 °C | 173 BTU-in/hr-ft²-°F @Temperature 212 °F |
| 28.7 W/m-K @Temperature 500 °C | 199 BTU-in/hr-ft²-°F @Temperature 932 °F |
Melting Point | 1480 - 1530 °C | 2700 - 2790 °F |
Solidus | 1480 °C | 2700 °F |
Liquidus | 1530 °C | 2790 °F |
Maximum Service Temperature, Air | 675 °C | 1250 °F |
| 760 °C | 1400 °F |
|
Component Elements Properties | Metric | English | Comments |
---|
Carbon, C | <= 0.15 % | <= 0.15 % |
Chromium, Cr | 13 % | 13 % |
Iron, Fe | 84 % | 84 % |
Manganese, Mn | <= 1.25 % | <= 1.25 % |
Phosphorus, P | <= 0.060 % | <= 0.060 % |
Selenium, Se | >= 0.15 % | >= 0.15 % |
Silicon, Si | <= 1.0 % | <= 1.0 % |
Sulfur, S | <= 0.060 % | <= 0.060 % |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.