MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Elvacite® 2552 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2552 is a solid bead thermoplastic methacrylate copolymer intended for use in solvent based coating systems where high gloss and apparent depth of finish are important. This specially designed polymer is internally plasticized to resist cold cracking and crazing and to provide flexibility over a broad range of temperatures. Elvacite® 2552 exhibits excellent outdoor durability and resistance to ultraviolet degradation and chemical attack from solvents such as alcohol or gasoline.

The resin may be used in refinish applications and transportation finishes such as automotive, motorcycle, and bicycle in multiple coats as a high gloss clear top coat, or as the main binder in high gloss glamour type pigmented base coats. Elvacite® 2552 demonstrates excellent adhesion to plastic substrates such as PS, ABS, and PVC as well as interlayer integrity and adhesion in multiple coat applications used to achieve depth. Solvent systems containing alcohol, methyl ethyl ketone, and toluene work well with Elvacite® 2552 whether the coating is applied mechanically or as an aerosol.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Density 1.079 g/cc0.03898 lb/in³
Brookfield Viscosity  1100 cP
@Temperature 25.0 °C
1100 cP
@Temperature 77.0 °F
in Toluene, 37.5% solids
 2250 cP
@Temperature 25.0 °C
2250 cP
@Temperature 77.0 °F
in Toluene, 40.0% solids
Viscosity Measurement 0.330.33Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 75000 g/mol75000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 15.515.5Tukon Hardness
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 90.0 °C194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® WSF-1121 Foam
Overview of materials for Acrylic, Optical Grade, Molded
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
Röhm Acrylite® H10 Acrylic molding and extrusion compound
Röhm XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound

PLUCIT9466 / 150180

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.