MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-FORM 5537 EMI Shielding Material
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-plated graphite particles dispersed in a silicone elastomer.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.20 g/cc2.20 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240
Tensile Strength at Break >= 1.38 MPa>= 200 psiASTM D412
Compression Set 50 %50 %ASTM D395 Method B 22 hrs 85°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.020 ohm-cm0.020 ohm-cmInitial; Chomerics MAT-1002
 0.030 ohm-cm0.030 ohm-cmAged; Chomerics MAT-1002
 
Processing PropertiesMetricEnglishComments
Cure Time 2880 min48.0 hourFull Cure
 >= 240 min
@Temperature 20.0 °C
>= 4.00 hour
@Temperature 68.0 °F
Minimum Cure time before inspection @ 50% RH
 
Descriptive Properties
Compression/Deflection @ 20%, N/cm2.1
Compression/Deflection @ 30%, N/cm4.8
FillerNi/C
ResinOne Part Silicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer

PCHOME088 / 28310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.