MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and corrosion resistance are needed.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 - 2.35 g/cc1.85 - 2.35 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 7050 - 70ASTM D2240
Tensile Strength at Break >= 1.03 MPa>= 150 psi
Elongation at Break 100 %100 %
Tear Strength 6.132 kN/m34.99 pli
Compression Set <= 40 %<= 40 %ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.10 ohm-cm0.10 ohm-cm
 0.25 ohm-cm0.25 ohm-cmAged; CEPS-0002
Shielding Effectiveness >= 95 dB>= 95 dB2 GHz (Plane Wave); MIL-G-83528
 >= 95 dB>= 95 dB10 GHz (Plane Wave); MIL-G-83528
 >= 100 dB>= 100 dB100 MHz (E Field); MIL-G-83528
 >= 100 dB>= 100 dB500 MHz (E Field); MIL-G-83528
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
Flammability, UL94 V-0
@Thickness 0.356 mm
V-0
@Thickness 0.0140 in
 
Descriptive Properties
BinderSilicone

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer
Parker Chomerics CHO-SEAL 1356 Conductive Elastomer
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer
Parker Chomerics CHO-FORM 5537 EMI Shielding Material

PCHOME135 / 28357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.