MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NDZ-S, UNS C99500, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: Same as C99400, but where higher yield strength is required.

Properties for as-sand-cast separately cast test bars(M01 temper). Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 503000 kg
 145500 kg
Tensile Strength, Ultimate >= 483 MPa
Tensile Strength, Yield >= 275 MPa
Elongation at Break >= 12 %in 50 mm
Tensile Modulus 19000 ksi
Machinability 50 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000012585 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.30 µin/in-°F
@Temperature 20.0 - 300 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 315 °CStress-Relieving Temperature
Precipitation Temperature 900 °F
@Time 3600 sec
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 - 2.0 %
Copper, Cu 87.9 %
Iron, Fe 3.0 - 5.0 %
Lead, Pb <= 0.25 %
Manganese, Mn <= 0.50 %
Nickel, Ni 3.5 - 5.5 %
Silicon, Si 0.50 - 2.0 %
Zinc, Zn 0.50 - 2.0 %
 
Descriptive Properties
Proportional Limit145 MPa

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy
Nondezincification Alloy, UNS C99400, Copper Casting Alloy
UNS C99300, Copper Casting Alloy
Leaded Nickel Brass, UNS C97300, Copper Casting Alloy
Aluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy

MC99500b1 / 11985

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.