MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell AP Armaflex® Through 1 1/2" & 2" Sheet and Roll Insulation
Categories: Other Engineering Material

Material Notes: The original, fiber-free, flexible elastomeric pipe, valve and duct insulation for reliable protection against condensation, mold and energy loss. AP Armaflex FS is PVC free.
  • Fiber free, formaldehyde-free, low VOC and non-particulating formulation protects indoor air quality
  • Closed-cell structure provides excellent condensation control
  • Built-in vapor barrier eliminates need for additional vapor retarder
  • Microban® antimicrobial product protection inhibits the growth of mold and mildew in the insulation
  • 25/50 rated for use in air plenums up to 1" thickness in AP Armaflex and 1-1/2" and 2" thickness in AP Armaflex FS
  • Thickness up to 2” with R-value up to R-8

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %ASTM C209
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0360 W/m-K
@Temperature 24.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
ASTM C177 or C518
Insulation R Value  1.60
@Thickness 9.52 mm
1.60
@Thickness 0.375 in
 2.10
@Thickness 12.7 mm
2.10
@Thickness 0.500 in
 3.10
@Thickness 19.0 mm
3.10
@Thickness 0.750 in
 4.20
@Thickness 25.4 mm
4.20
@Thickness 1.00 in
 6.00
@Thickness 38.1 mm
6.00
@Thickness 1.50 in
 8.00
@Thickness 50.8 mm
8.00
@Thickness 2.00 in
Maximum Service Temperature, Air 105 °C221 °FASTM C534
Minimum Service Temperature, Air -183 °C-297 °FASTM C534
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Water Vapor Permeability0.08 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
INEOS Styrolution Luran® 368R Crystal Clear Transparent 77851 SAN
Chemours Viton® Extreme™ ETP-600S Fluoroelastomer Compound
Armacell AP Armaflex® SA Through 1" Self-Adhering Sheet & Roll Insulation

PARMD021 / 186632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.