MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, communications (bobbin, relay bed, optical cable closure), military, sports equipment (skis, helmets, foot wear), and medical equipment. Product is customizable.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Filler Content 40 %Glass Fiber
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 126 MPaASTM D638
Elongation at Break 2.4 %ASTM D638
Flexural Strength 170 MPaASTM D790
Flexural Modulus 7.60 GPaASTM D790
Izod Impact Resistance 2.60 J/cm²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 160 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 216 - 232 °C
Middle Barrel Temperature 210 - 227 °C
Front Barrel Temperature 204 - 221 °C
Melt Temperature 210 - 249 °C
Mold Temperature 38.0 - 77.0 °C
Injection Velocity 13.0 - 25.0 mm/sec
Injection Pressure 69.0 - 103 MPa
Hold Pressure 34.0 - 69.0 MPa
Back Pressure 0.170 - 0.340 MPa
Screw Speed 30 - 70 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® PP GF40 CC 40% Glass Filled
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene
Hanwha Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)

PZHEJ001 / 92816

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.