MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Bioline High-N Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik Bioline High-N is a Molybdenum and Nitrogen alloyed austenitic stainless steel with a proof strength up to twice that of Sandvik 316LVM, high corrosion resistance and cleanliness. Used for orthopedic implants and fracture fixation devices.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 250250Annealed
 360360Medium Tensile
 400400High Tensile
Tensile Strength, Ultimate 740 MPa107000 psiTube, thick wall, Bright annealed
 740 MPa107000 psiBar, Annealed
 1000 MPa145000 psiBar, medium
 1100 MPa160000 psiBar, Hard
 1200 MPa174000 psiTube, thick wall, Cold finished
 <= 1500 MPa<= 218000 psiWire
Tensile Strength, Yield  430 MPa
@Strain 0.2 %
62400 psi
@Strain 0.2 %
Bar, Annealed
 430 MPa
@Strain 0.2 %
62400 psi
@Strain 0.2 %
Tube, thick wall, Bright annealed
 700 MPa
@Strain 0.2 %
102000 psi
@Strain 0.2 %
Bar, Medium
 1000 MPa
@Strain 0.2 %
145000 psi
@Strain 0.2 %
Bar, Hard
 1100 MPa
@Strain 0.2 %
160000 psi
@Strain 0.2 %
Tube, thick wall, Cold finished
Elongation at Break >= 15 %>= 15 %Bar, Hard
 >= 20 %>= 20 %Bar, Medium
 >= 40 %>= 40 %Bar, Annealed
 >= 40 %>= 40 %Tube, thick wall, Bight annealed
Modulus of Elasticity 200 GPa29000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
9.17 µin/in-°F
@Temperature 86.0 - 212 °F
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
0.116 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Chromium, Cr 20.5 %20.5 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe 62 %62 %As Balance
Manganese, Mn 4.0 %4.0 %
Molybdenum, Mo 2.4 %2.4 %
Nickel, Ni 9.5 %9.5 %
Niobium, Nb (Columbium, Cb) 0.30 %0.30 %
Nitrogen, N 0.40 %0.40 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.60 %<= 0.60 %
Sulfur, S <= 0.0030 %<= 0.0030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Aluminum - SiC Metal Matrix Composite
Medical Grade Stainless Steel 316LVM
Overview of materials for AISI 8000 Series Steel
Sandvik 303-6RA11 Billet

NSANDV139 / 19033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.