MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Bioline High-N Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik Bioline High-N is a Molybdenum and Nitrogen alloyed austenitic stainless steel with a proof strength up to twice that of Sandvik 316LVM, high corrosion resistance and cleanliness. Used for orthopedic implants and fracture fixation devices.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 250Annealed
 360Medium Tensile
 400High Tensile
Tensile Strength, Ultimate 740 MPaTube, thick wall, Bright annealed
 740 MPaBar, Annealed
 1000 MPaBar, medium
 1100 MPaBar, Hard
 1200 MPaTube, thick wall, Cold finished
 <= 1500 MPaWire
Tensile Strength, Yield 430 MPa
@Strain 0.2 %
Bar, Annealed
 430 MPa
@Strain 0.2 %
Tube, thick wall, Bright annealed
 700 MPa
@Strain 0.2 %
Bar, Medium
 1000 MPa
@Strain 0.2 %
Bar, Hard
 1100 MPa
@Strain 0.2 %
Tube, thick wall, Cold finished
Elongation at Break >= 15 %Bar, Hard
 >= 20 %Bar, Medium
 >= 40 %Bar, Annealed
 >= 40 %Tube, thick wall, Bight annealed
Modulus of Elasticity 200 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.060 %
Chromium, Cr 20.5 %
Copper, Cu <= 0.20 %
Iron, Fe 62 %As Balance
Manganese, Mn 4.0 %
Molybdenum, Mo 2.4 %
Nickel, Ni 9.5 %
Niobium, Nb (Columbium, Cb) 0.30 %
Nitrogen, N 0.40 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.60 %
Sulfur, S <= 0.0030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Aluminum - SiC Metal Matrix Composite
Medical Grade Stainless Steel 316LVM
Overview of materials for AISI 8000 Series Steel
Sandvik 303-6RA11 Billet

NSANDV139 / 19033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.