Product Description: Weston™ 398T phosphate is a versatile phosphate stabilizer which is useful in a large number of polymers such as HDPE, LLDPE, SBR, ABS, PVC and others. Features: - Low color and low nonylphenol content
- Improves color and processing stability during recovery, drying, compounding, processing and end use
- Synergism is realized when this product is combined with other stabilizers such as hindered phenols.
- May be added alone or in combination with the monomers and/or in antioxidant emulsions during recovery and/or during compounding
Application: Weston™ 398T phosphite is a versatile liquid phosphite stabilizer which improves color and processing stability as well as end use of a variety of polymers such as HDPE, LLDPE, SBR, ABS, PVC and others.CAS No: 26523-78-4 Information provided by Akrochem Corporation |