MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Akrochem Weston™ 398T Antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Weston™ 398T phosphate is a versatile phosphate stabilizer which is useful in a large number of polymers such as HDPE, LLDPE, SBR, ABS, PVC and others.

Features:

  • Low color and low nonylphenol content
  • Improves color and processing stability during recovery, drying, compounding, processing and end use
  • Synergism is realized when this product is combined with other stabilizers such as hindered phenols.
  • May be added alone or in combination with the monomers and/or in antioxidant emulsions during recovery and/or during compounding
Application: Weston™ 398T phosphite is a versatile liquid phosphite stabilizer which improves color and processing stability as well as end use of a variety of polymers such as HDPE, LLDPE, SBR, ABS, PVC and others.

CAS No: 26523-78-4

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 0.992 g/cc0.980 - 0.992 g/cc
Viscosity 250 cP
@Temperature 60.0 °C
250 cP
@Temperature 140 °F
Molecular Weight 688 g/mol688 g/mol
Vapor Pressure <= 0.00800 bar
@Temperature 245 °C
<= 6.00 torr
@Temperature 473 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.25<= 0.25[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.67 J/g-°C0.399 BTU/lb-°F
Thermal Conductivity 0.126 W/m-K0.870 BTU-in/hr-ft²-°F
Flash Point 196 °C385 °FPensky-Martens Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.525 - 1.5281.525 - 1.528
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 4.1 - 4.5 %4.1 - 4.5 %
 
Descriptive Properties
AppearanceClear liquid
Color<75Pt - Co
Content<0.5%Free Nonylphenol
 <25 ppmChlorine
 <50 ppmFree Phenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH514 / 315432

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.